Datasheet: MP35N

MP35N

MP35N is an age hardenable Nickel-Cobalt base alloy that has a unique combination of properties – ultra high strength, toughness, ductility and outstanding corrosion resistance. MP35N resists corrosion in hydrogen sulphide, salt water and other chloride solutions. It also has excellent resistance to crevice and stress corrosion cracking in sea water and other hostile environments.

The four alloy elements in MP35N are the basis for corrosion resistance in almost every Stainless Steel, Nickel and Cobalt-based alloy commonly used in the industry. The alloy resists corrosion in hydrogen sulphide, salt water and other Chloride solutions, as well as the mineral acids (Nitric, Hydrochloric and Sulphuric).

MP35N is suitable where a high combination of strength, high modulus values and good corrosion resistance are required.

Applications for this alloy also include medical devices and dental products.

Available in all profile options

MP35N - Alloy Wire International 1

Key Features

MP35N offers the following key features:

Combination of high strength, ductility and good mechanical properties at ambient temperatures.
Excellent corrosion resistance in hydrogen sulphide.
Excellent resistance to crevice and stress corrosion cracking in sea water.
Age hardenable (Spring Temper only).

Typical Applications

MP35N is known to be suitable for the following applications:

Medical Devices
Marine Engineering


Designations

W. Nr. 2.4999
UNS R30035
AWS 110

Specifications

AMS 5844
AMS 5845
ASTM F562
ISO 15156-3
(NACE MR 0175)
ISO 5832-6

Chemical Composition

The chemical composition of MP35N is indicated in the table below:

ElementMin %Max %
C0.025
P0.015
Si0.15
Ni33.0037.00
Cobal 
Mn0.15
S0.01
Cr19.0021.00
Mo9.0010.50
Ti1.00
Fe1.00

Alloy Details

MP35N density, melting point, coefficient of expansion, and modulus of elasticity is indicated in the table below:

DensityMelting PointCoefficient of ExpansionModulus of RigidityModulus of Elasticity
8.43 g/cm³1440 °C12.8 μm/m °C (20 – 100 °C)80.7 kN/mm²234 kN/mm²
0.304 lb/in³2625 °F7.1 x 10-6 in/in °F (70 – 212 °F)11705 ksi33939 ksi

Heat treatment of finished parts

The typical heat treatment of MP35N:

Condition as supplied by AWITypeTemperatureTimeCooling
Annealed
Spring TemperAge Harden650 °C (1200 °F)4 HrAir

Properties

The typical heat treatment of MP35N:

Annealed
Approx. tensile strength< 1100 N/mm²< 160 ksi
Approx. operating temperature-200 to +315 °C-330 to +600 °F
Spring Temper
Approx. tensile strength1400 – 1900 N/mm²203 – 276 ksi
Approx. operating temperature-200 to +315 °C-330 to +600 °F
Spring Temper + Aged
Approx. tensile strength1900 – 2200 N/mm²276 – 319 ksi
Approx. operating temperature-200 to +315 °C-330 to +600 °F

The above tensile strength ranges are typical. If you require different please ask.