New Alloy: Inconel® 617 is now available from Alloy Wire. Learn about Inconel® 617
Datasheet: Monel® 400
A Nickel-Copper alloy with high strength and excellent corrosion resistance in a range of acidic and alkaline environments and suitable for reducing conditions. It also has good ductility and thermal conductivity. Used in a variety of applications, Monel® 400 has excellent resistance to seawater, and can also be used in hydrochloric and hydrofluoric acids.
Monel® 400 is also known as Phyweld 400 and Nicorros LC.
Available in all profile options
Monel® 400 offers the following key features:
Excellent corrosion resistance in a wide range of acidic & alkaline environments
Especially suitable for reducing conditions
Good ductility & thermal conductivity
Good for sea water applications
Monel® 400 is known to be suitable for the following applications:
Marine engineering
Chemical processing
Hydro-carbon processing
Heat exchangers
Valves
Pumps
W.Nr 2.4361
W.Nr 2.4360
UNS N04400
AWS 040
AMS 4730
ASTM B164
BS 3075 NA 13
BS 3076 NA 13
DTD 204B
ISO 15156-3
(NACE MR 0175)
QQ-N-281
The chemical composition of Monel® 400 is indicated in the table below:
Element | Min % | Max % |
---|---|---|
C | – | 0.3 |
Si | – | 0.50 |
Mn | – | 2.00 |
S | – | 0.024 |
Cu | 28.00 | 34.00 |
Fe | – | 2.50 |
Ni+Co | 63.00 | 70.00 |
Co | – | 2.0 |
Monel® 400 density, melting point, coefficient of expansion, modulus of rigidity, and elasticity is indicated in the table below:
Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
---|---|---|---|---|
8.8 g/cm³ | 1350 °C | 13.9 μm/m °C (20 – 100 °C) | 65.3 kN/mm² | 173 kN/mm² |
0.318 lb/in³ | 2460 °F | 7.7 x 10-6 in/in °F (70 – 212 °F) | 9471 ksi | 25092 ksi |
The typical heat treatment of Monel® 400:
Condition as supplied by AWI | Type | Temperature | Time | Cooling |
---|---|---|---|---|
Annealed or Spring Temper | Stress Relieve | 300 – 320 °C (570 – 610 °F) | 0.5 – 1 Hr | Air |
The typical mechanical properties of Monel® 400:
Annealed | ||
---|---|---|
Approx. tensile strength | <600 N/mm² | <87 ksi |
Approx. operating temperature | -200 to +230 °C | -330 to +445 °F |
Spring Temper | ||
---|---|---|
Approx. tensile strength | 800 – 1100 N/mm² | 116 – 160 ksi |
Approx. operating temperature | -200 to +230 °C | -330 to +445 °F |
The above tensile strength ranges are typical. If you require different please ask.
*Trade name of Special Metals Group of Companies